This search combines search strings from the content search (i.e. "Full Text", "Author", "Title", "Abstract", or "Keywords") with "Article Type" and "Publication Date Range" using the AND operator.
Beilstein J. Nanotechnol. 2015, 6, 907–918, doi:10.3762/bjnano.6.94
Figure 1: In situ EDS spectra of deposits purified using an electron beam with an energy of 5 keV, a current ...
Figure 2: a) Cross-section SEM images of 400 nm thick PtCx deposits that were purified for 1, 2, 4, 6, 8, and...
Figure 3: Normalized carbon peak area plotted as a function of a) curing time for the indicated pixel resolut...
Figure 4: a) Normalized carbon peak area plotted as a function of dose for the beam energies shown. b) Monte ...
Figure 5: a) Images of wire deposits with different initial thicknesses (wires 1–4) purified at 1 min interva...
Figure 6: a) EDS measurements of the samples deposited and purified on the TEM membranes. TEM images of an b)...
Figure 7: Selected area electron diffraction (SAED) patterns for O2 E-beam uncured (left) and cured (right) d...
Figure 8: Bar graph comparing the simulated and experimental purification rates for varying beam parameters.